Axiall 4590 Flexible PVC

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Axiall
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 4590 Flexible PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
10 mil automotive thin wall insulation.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.29 - 1.33 g/cc
1.29 - 1.33 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore D 56 - 62
56 - 62
delayed; ASTM D-2240
Tensile Strength, Yield 24.5 MPa
3550 psi
ASTM D-638
Elongation at Yield 260 %
260 %
ASTM D-638
100% Modulus 0.0217 GPa
3.15 ksi
ASTM D-638
Thermal Properties Metric English Comments
Brittleness Temperature -12.0 °C
10.4 °F
ASTM D-746
Processing Properties Metric English Comments
Melt Temperature 193 °C
380 °F