Axiall 48562 Moldings & Extrusions Flexible PVC

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Axiall
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 48562 Moldings & Extrusions Flexible PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Automotive window encapsulation compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.33 - 1.37 g/cc
1.33 - 1.37 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore A 75 - 81
75 - 81
delayed; ASTM D-2240
81 - 87
81 - 87
ASTM D-2240
Tensile Strength, Yield 13.8 MPa
2000 psi
ASTM D-638
Elongation at Yield 300 %
300 %
ASTM D-638