Material Notes:
Non-lead stabilized, 105°C rated vinyl elastomer compound suitable for SJEOW insulation and jacket applications per UL 62. UL, QMTT2 recognized for 720 hour sunlight resistance applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.24 - 1.28 g/cc
1.24 - 1.28 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore A 74 - 80
74 - 80
delayed; ASTM D-2240
Tensile Strength, Yield 14.5 MPa
2100 psi
ASTM D-638
Elongation at Yield 232.1 %
232.1 %
Oil Aging: 168 hours @ 60°C; #2 Oil; 30 mil slabs; UL 1581
236.5 %
236.5 %
Air Aging: 168 hours @ 136°C; 30 mil slabs; UL 1581
275 %
275 %
ASTM D-638
100% Modulus 0.00758 GPa
1.10 ksi
ASTM D-638
Thermal Properties Metric English Comments
Brittleness Temperature -45.0 °C
-49.0 °F
ASTM D-746
Oxygen Index 24 %
24 %
ASTM D-638
Processing Properties Metric English Comments
Melt Temperature 188 °C
370 °F