Axiall 7181 Rigid PVC, Extrusion

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Axiall
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 7181 Rigid PVC, Extrusion.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Georgia Gulf 7181 is a special purpose rigid PVC profile extrusion compound designed for applications requiring the following properties: WeatherabilityImpact StrengthDimensional StabilityFlame RetardantChemical ResistanceInformation provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.42 g/cc
1.42 g/cc
ASTM D-792
Linear Mold Shrinkage 0.0020 - 0.0030 cm/cm
0.0020 - 0.0030 in/in
ASTM D-955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 112
112
ASTM D-785
Hardness, Shore D 80
80
ASTM D-2240
Tensile Strength, Yield 42.1 MPa
6100 psi
ASTM D-638
Tensile Modulus 2.48 GPa
360 ksi
ASTM D-638
Flexural Strength 75.8 MPa
11000 psi
ASTM D-790
Flexural Modulus 2.83 GPa
410 ksi
ASTM D-790
Izod Impact, Notched 9.61 J/cm
18.0 ft-lb/in
ASTM D-256
Tensile Impact Strength 158 kJ/m²
75.0 ft-lb/in²
ASTM D-1822
Dart Drop Total Energy 53.4 J/cm
0.100 ft-lb/mil
23°C, C.125 Tup, Method A; ASTM D-4226
Thermal Properties Metric English Comments
CTE, linear 63.0 µm/m-°C

@Temperature 20.0 °C
35.0 µin/in-°F

@Temperature 68.0 °F
ASTM D-696
Deflection Temperature at 1.8 MPa (264 psi) 72.2 °C
162 °F
ASTM D-648
Flammability, UL94 V-0
V-0
Descriptive Properties Value Comments
Cell Classification 14413233
ASTM D-4216
Color Values: ?L=±1.0, ?a=±0.5, ?b=±0.5