Material Notes:
Georgia Gulf 7407 is a rigid PVC compound designed for outdoor applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.50 g/cc
1.50 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore D 76
76
ASTM D-2240
Tensile Strength, Yield 40.7 MPa
5900 psi
ASTM D-638
Tensile Modulus 3.09 GPa
448 ksi
ASTM D-638
Flexural Strength 77.9 MPa
11300 psi
ASTM D-790
Flexural Modulus 2.45 GPa
356 ksi
ASTM D-790
Izod Impact, Notched 2.03 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
3.80 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D-256
Tensile Impact Strength 168 kJ/m²
80.0 ft-lb/in²
ASTM D-1822
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 68.9 °C
156 °F
ASTM D-648
Processing Properties Metric English Comments
Melt Temperature 182 °C
360 °F