Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Axiall 7751 Rigid PVC, Extrusion

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Axiall
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 7751 Rigid PVC, Extrusion.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Georgia Gulf 7751 is a vertical blind profile exterior compound requiring the following properties: Impact Strength & ToughnessColorabilityDimensional StabilityUV Color StabilityEasy Processing in Thin Parts at Fast RatesInformation provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.50 g/cc
1.50 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Rockwell R 111.9
111.9
ASTM D-785
Hardness, Shore D 81
81
ASTM D-2240
Tensile Strength, Yield 40.5 MPa
5870 psi
ASTM D-638
Tensile Modulus 3.22 GPa
467 ksi
ASTM D-638
Flexural Strength 74.19 MPa
10760 psi
ASTM D-790
Flexural Modulus 3.07 GPa
445 ksi
ASTM D-790
Izod Impact, Notched 1.44 J/cm

@Thickness 6.35 mm
2.70 ft-lb/in

@Thickness 0.250 in
ASTM D-256
2.14 J/cm

@Thickness 3.17 mm
4.00 ft-lb/in

@Thickness 0.125 in
ASTM D-256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 69.50 °C
157.1 °F
ASTM D-648
Users viewing this material also viewed the following: