General purpose, jelly clear flexible PVC compound recommended for extrusion or molding applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.14 - 1.18 g/cc
1.14 - 1.18 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore A 52 - 58
52 - 58
delayed; ASTM D-2240
Tensile Strength, Yield 8.27 MPa
1200 psi
ASTM D-638
Elongation at Yield 500 %
500 %
ASTM D-638
100% Modulus 0.00241 GPa
0.350 ksi
ASTM D-638
Processing Properties Metric English Comments
Melt Temperature 160 °C
320 °F