Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Axiall 9109J Clear Rigid PVC, Extrusion, Clear

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Axiall
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 9109J Clear Rigid PVC, Extrusion, Clear.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Georgia Gulf 9109J Clear is designed for use in extruded price tag holders. The compound contains an ultraviolet light stabilizer, which retards color change.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.34 g/cc
1.34 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore D 75
75
ASTM D-2240
Tensile Strength, Yield 46.2 MPa
6700 psi
ASTM D-638
Tensile Modulus 2.48 GPa
360 ksi
ASTM D-638
Flexural Strength 82.7 MPa
12000 psi
ASTM D-790
Flexural Modulus 2.41 GPa
350 ksi
ASTM D-790
Izod Impact, Notched 5.34 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
10.0 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D-256
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
clear; thickness not quantified
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved