Material Notes:
Georgia Gulf ProTherm® 4351 is a CPVC powder blend designed for extrusion of large diameter, heavy wall industrial grade pipe requiring high heat deflection temperatures and excellent chemical resistance. Processing and stability with overall physical properties are excellent. Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.50 g/cc
1.50 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Rockwell R 116
116
ASTM D-785
Hardness, Shore D 82
82
ASTM D-2240
Tensile Strength, Yield 51.7 MPa
7500 psi
ASTM D-638
Elongation at Yield 4.0 %
4.0 %
ASTM D-638
Tensile Modulus 2.68 GPa
389 ksi
ASTM D-638
Flexural Strength 82.7 MPa
12000 psi
ASTM D-790
Flexural Modulus 2.13 GPa
309 ksi
ASTM D-790
Izod Impact, Notched 2.30 J/cm

@Thickness 6.35 mm
4.30 ft-lb/in

@Thickness 0.250 in
ASTM D-256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 106 °C
222 °F
unannealed; ASTM D-648
112 °C
233 °F
annealed; ASTM D-648
Deflection Temperature at 1.8 MPa (264 psi) 106 °C
222 °F
annealed; ASTM D-648
Descriptive Properties Value Comments
Cell Classification 23447
ASTM D-1784
Fusion Temperature, °C 208
ASTM D-2538
Fusion Time, minutes 2
ASTM D-2538
Fusion Torque, meter-grams 4000
ASTM D-2538
Line-Out Temperature, °C 220
ASTM D-2538
Minimum Torque, meter-grams 2750
ASTM D-2538
Total Dynamic Thermal Stability, minutes 20
ASTM D-2538