Material Notes:
Georgia Gulf SP-7008 is a rigid vinyl compound formulated for electrical fittings and molded parts requiring high impact strength and toughness.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.33 g/cc
1.33 g/cc
ASTM D-792
Linear Mold Shrinkage 0.0030 - 0.0050 cm/cm
0.0030 - 0.0050 in/in
ASTM D-955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 105
105
ASTM D-785
Tensile Strength, Yield 41.4 MPa
6000 psi
ASTM D-638
Tensile Modulus 2.48 GPa
360 ksi
ASTM D-638
Flexural Strength 68.9 MPa
10000 psi
ASTM D-790
Flexural Modulus 2.34 GPa
340 ksi
ASTM D-790
Izod Impact, Notched 0.801 J/cm

@Temperature 23.0 °C
1.50 ft-lb/in

@Temperature 73.4 °F
ASTM D-256
2.67 J/cm

@Temperature -20.0 °C
5.00 ft-lb/in

@Temperature -4.00 °F
ASTM D-256
Gardner Impact 36.2 J

@Temperature 23.0 °C
26.7 ft-lb

@Temperature 73.4 °F
1/2" R Tup, 123 mil
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 70.0 °C
158 °F
ASTM D-648
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °C
149 °F
ASTM D-648
Flammability, UL94 V-0
V-0
Oxygen Index 36 %
36 %
ASTM D-2863
Descriptive Properties Value Comments
Flow Ratio (Distance/Wall Thickness, 390-400°F) 130
Georgia Gulf Test