Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Axion Polymers Axpoly® PS01 Impact Modified Polystyrene

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Impact Modified
Manufacturer Axion Polymers
Trade Name Axpoly®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axion Polymers Axpoly® PS01 Impact Modified Polystyrene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
100% post-consumer recycled polymer (recovered from refrigerators)93% less CO2 impact compared with virgin*Successfully replaces virgin grade resinISO9000 quality certifiedAvailable in a range of colorsCost savings compared with virgin polymer gradesPrevious applications include washing machine parts, horticultural pots, and television partsInformation provided by Axion Recycling
Physical Properties Metric English Comments
Density 1.03 - 1.05 g/cc
0.0372 - 0.0379 lb/in³
Typical; ISO 1183-1
1.03 - 1.06 g/cc
0.0372 - 0.0383 lb/in³
Spec; ISO 1183-1
Particle Size 2000 - 4000 µm
2000 - 4000 µm
Pellet Size
3000 µm
3000 µm
Typical
Melt Index of Compound 6.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
6.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
Typical
5.0 - 8.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
5.0 - 8.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
Spec
Mechanical Properties Metric English Comments
Tensile Strength, Yield 15.0 - 25.0 MPa
2180 - 3630 psi
Spec; ISO 527-1/2
21.0 - 22.0 MPa
3050 - 3190 psi
Typical; ISO 527-1/2
Elongation at Break 35 %
35 %
Typical; ISO 527 - 1/2
25 - 50 %
25 - 50 %
Spec; ISO 527 - 1/2
Izod Impact, Unnotched (ISO) 6.00 - 10.0 kJ/m²
2.86 - 4.76 ft-lb/in²
Spec; ISO 180
8.00 kJ/m²
3.81 ft-lb/in²
Typical; ISO 180
Processing Properties Metric English Comments
Moisture Content 0.17 %
0.17 %
Typical
<= 0.25 %
<= 0.25 %
Spec
Copyright © lookpolymers.com All Rights Reserved