Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Azdel Plus C321-B01 32% Chopped Fiber Mat / PP Resin Matrix

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Azdel
Trade Name Plus
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Azdel Plus C321-B01 32% Chopped Fiber Mat / PP Resin Matrix.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AZDEL® C321-B01 is a glass mat thermoplastic laminate based upon a random oriented chopped fiber mat contained within a polypropylene resin matrix. This composite material features high flow properties and a very homogeneous fiber distribution. This material is typically used for standard semi-structural thin wall applications and where good glass distributions into features such as ribs and bosses is desired.Mechanical properties and mold shrinkage measured on flat plaques.Information provided by Azdel.
Physical Properties Metric English Comments
Specific Gravity 1.12 g/cc
1.12 g/cc
Laminate; ASTM D792
1.14 g/cc
1.14 g/cc
Molded; ASTM D792
Filler Content 32 %
32 %
By weight (ashing); Internal
Thickness 3600 microns
142 mil
Sheet; Internal
Linear Mold Shrinkage 0.0010 - 0.0030 cm/cm
0.0010 - 0.0030 in/in
Measured on flat plaques; ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 76.0 MPa
11000 psi
ISO 527
Elongation at Break 2.4 %
2.4 %
ISO 527
Tensile Modulus 4.62 GPa
670 ksi
ISO 527
Flexural Strength 104 MPa
15100 psi
ISO 178
Flexural Modulus 4.574 GPa
663.4 ksi
ISO 178
Poissons Ratio 0.317
0.317
ISO 527
Izod Impact, Notched 5.60 J/cm

@Thickness 4.00 mm,
Temperature 23.0 °C
10.5 ft-lb/in

@Thickness 0.157 in,
Temperature 73.4 °F
ISO 180
Impact 220

@Thickness 4.00 mm
220

@Thickness 0.157 in
Multi-axial in kg, at max. load; ASTM D3763
Impact Test 9.00 J

@Thickness 4.00 mm
6.64 ft-lb

@Thickness 0.157 in
Multi-axial, at max. load; ASTM D3763
18.0 J

@Thickness 4.00 mm
13.3 ft-lb

@Thickness 0.157 in
Multi-axial, at failure; ASTM D3763
Thermal Properties Metric English Comments
CTE, linear 36.0 µm/m-°C

@Temperature -40.0 - 120 °C
20.0 µin/in-°F

@Temperature -40.0 - 248 °F
ASTM E831
Deflection Temperature at 1.8 MPa (264 psi) 151 °C
304 °F
ASTM D648
Flame Spread 5.08 mm/min
0.200 in/min
FMVSS302
Descriptive Properties Value Comments
Color Black
Internal