Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

BACT DLC Diamond-Like Coating

Category Carbon , Diamond , Other Engineering Material , Ceramic/Metallic Coating
Manufacturer Bekaert Advanced Coating Technologies (BACT)
Trade Name DLC
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BACT DLC Diamond-Like Coating.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DLC (a-C:H). This coating provides the highest hardness and abrasion resistance of the BACT products. Typical applications include high wear environments involving seals, molds, metal forming, and powder compaction.Applied using a PACVD (plasma-assisted physical vapor deposition) coating method. Diamond-like coatings are amorphous carbon-based coatings that exhibit high hardness and low coefficients of friction. Their unique composition and structure result in excellent wear resistance and non-stick characteristics. These coatings are thin, chemically inert, corrosion resistant, have minimal particulate contamination, tailorable electrical resistivities, and have a very low surface roughness.Information provided by Bekaert Advanced Coating Technologies (BACT).
Physical Properties Metric English Comments
Thickness 0.100 - 4.00 microns
0.00394 - 0.157 mil
Coating Thickness
Mechanical Properties Metric English Comments
Hardness, Rockwell C 77 - 82
77 - 82
Coefficient of Friction 0.10 - 0.20
0.10 - 0.20
Dry vs. Steel
K (wear) Factor 1.00 - 5.00 x 10-8 mm³/N-M
0.496 - 2.48 x 10-10 in³-min/ft-lb-hr
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 300 °C
572 °F
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+6 - 1.00e+12 ohm-cm
1.00e+6 - 1.00e+12 ohm-cm
Dielectric Strength 100 - 200 kV/mm
2540 - 5080 kV/in
Thickness up to 1 µm
Processing Properties Metric English Comments
Processing Temperature 150 - 200 °C
302 - 392 °F
Coating Temperature
Descriptive Properties Value Comments
Microhardness 18 - 25 GPa
Surface Energy 40 - 50 mN/m
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved