Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

BASF E-por® 0.035 g/cc Density; Styrene and Ethylene (Europe)

Category Polymer , Thermoplastic , Polyethylene (PE) , Polystyrene (PS) , Expanded Polystyrene (EPS)
Manufacturer BASF
Trade Name E-por®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF E-por® 0.035 g/cc Density; Styrene and Ethylene (Europe).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Expandable granules made of styrene and ethylene containing polymers without flame retardant (blowing agent: pentane).Application: For the production of elastic, multi-shock absorbing expanded foams.Information provided by BASF
Physical Properties Metric English Comments
Bulk Density 0.0160 - 0.0350 g/cc
0.000578 - 0.00126 lb/in³
Density 0.0350 g/cc
0.00126 lb/in³
Mechanical Properties Metric English Comments
Flexural Strength 0.237 MPa
34.4 psi
0% E-por Content; DIN 53423
0.247 MPa
35.8 psi
60% E-por Content; DIN 53423
0.257 MPa
37.3 psi
100% E-por Content; DIN 53423
0.480 MPa
69.6 psi
DIN-EN 12089
Compressive Strength 0.165 MPa

@Strain 10.0 %
23.9 psi

@Strain 10.0 %
DIN-EN 826
0.205 MPa

@Strain 25.0 %
29.7 psi

@Strain 25.0 %
DIN-EN 826
Processing Properties Metric English Comments
Moisture Content <= 0.50 %
<= 0.50 %
Descriptive Properties Value Comments
Commercial Status Europe
Cushioning 2.65
h/d=15; DIN 55471
Energy Absorption 19 J
Hysteresis at 70% compression, v=% mm/min; ISP 3386-1
Flexural Work to Break 0.227
0% E-por Content; DIN 53423
0.247
60% E-por Content; DIN 53423
0.25
100% E-por Content; DIN 53423
7.4 J
DIN-EN 12098
Copyright © lookpolymers.com All Rights Reserved