BASF Elastollan 1154 D FHF TPUR Flame Retardant Halogen Free

Category Polymer , Thermoplastic , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyether Grade
Manufacturer BASF
Trade Name Elastollan
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Elastollan 1154 D FHF TPUR Flame Retardant Halogen Free.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Thermoplastic Polyether Polyurethane Elastomers with outstanding hydrolysis resistance, low temperature flexibility and resistance to micro-organisms.Typical Applications: Cable sheathing, plugs and terminations, spiral tubing, films, ski boot shells, ear tags, technical moldings, e.g. mining screens, railway pads and seals.Note: Quoted results are from measurements on injection molded test platens, post tempered for 20 hours at 100°CInformation provided by BASF
Physical Properties Metric English Comments
Density 1.27 g/cc
0.0459 lb/in³
ISO 1183-1-A
Mechanical Properties Metric English Comments
Hardness, Shore D 58
58
ISO 686
Tensile Strength 20.0 MPa
2900 psi
after storage in water at 80°C for 42 days; ISO 37
30.0 MPa
4350 psi
ISO 37
13.0 MPa

@Strain 20.0 %
1890 psi

@Strain 20.0 %
ISO 37
19.0 MPa

@Strain 100 %
2760 psi

@Strain 100 %
ISO 37
33.0 MPa

@Strain 300 %
4790 psi

@Strain 300 %
ISO 37
Elongation at Break 400 %
400 %
ISO 37
400 %
400 %
after storage in water at 80°C for 42 days; ISO 37
Charpy Impact, Notched 0.300 J/cm²

@Temperature -30.0 °C
1.43 ft-lb/in²

@Temperature -22.0 °F
DIN EN ISO 179
5.00 J/cm²

@Temperature 23.0 °C
23.8 ft-lb/in²

@Temperature 73.4 °F
DIN EN ISO 179
Tear Strength 110 kN/m
628 pli
DIN ISO 34-1/Bb
Abrasion 30
30
[mm<sup>3</sup>; ISO 4649
Compression Set 30 %

@Temperature 23.0 °C
30 %

@Temperature 73.4 °F
ISO 815
45 %

@Temperature 70.0 °C
45 %

@Temperature 158 °F
ISO 815
Thermal Properties Metric English Comments
Flammability, UL94 V-2
V-2
according to wall section
V-0
V-0
Processing Properties Metric English Comments
Processing Temperature 160 - 220 °C
320 - 428 °F
Extrusion
170 - 240 °C
338 - 464 °F
Injection molding
Mold Temperature 20.0 - 70.0 °C
68.0 - 158 °F
Descriptive Properties Value Comments
Commercial Status North America
Primary Processing Technique Injection molding and Extrusion