BASF Elastollan® 1164D Polyether Type Polyurethane Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP , Thermoplastic Polyurethane, Elastomer, Ether Grade
Manufacturer BASF
Trade Name Elastollan®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Elastollan® 1164D Polyether Type Polyurethane Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Recommended for injection molding. Elastollan ® 1100 series products are FDA Sec. 177.2600 compliant. Elastollan 1100 series of products are polyether-based thermoplastic polyurethanes. They exhibit excellent low temperature properties, hydrolysis resistance and fungus resistance. These products can be injection and blow molded and extruded. As with all TPU products this grade must be dried prior to processing.Property values below are typical values based on test samples cured 20 hours at 100°C before testing. Information provided by BASF Corporation.
Physical Properties Metric English Comments
Density 1.18 g/cc
0.0426 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore D 64
64
ASTM D2240
Tensile Strength, Ultimate 41.0 MPa
5950 psi
ASTM D412
Tensile Strength, Yield 25.0 MPa

@Strain 100 %
3630 psi

@Strain 100 %
ASTM D-412
33.0 MPa

@Strain 300 %
4790 psi

@Strain 300 %
ASTM D-412
Elongation at Break 425 %
425 %
ASTM D412
Modulus of Elasticity 0.280 GPa
40.6 ksi
Shear Modulus 0.150 GPa
21.8 ksi
Tear Strength 220 kN/m
1260 pli
ASTM D624
Taber Abrasion, mg/1000 Cycles 55
55
H-18 wheel; ASTM D-1044.
Tensile Set 90 %
90 %
at break; ASTM D-412
Thermal Properties Metric English Comments
Vicat Softening Point 145 °C
293 °F
Electrical Properties Metric English Comments
Dielectric Constant 4.6

@Frequency 1e+6 Hz
4.6

@Frequency 1e+6 Hz
DIN 53483/VDE 0303
5.4

@Frequency 1000 Hz
5.4

@Frequency 1000 Hz
DIN 53483/VDE 0303
5.8

@Frequency 50 Hz
5.8

@Frequency 50 Hz
DIN 53483/VDE 0303
Dielectric Strength >= 49.0 kV/mm
>= 1240 kV/in
DIN 53481/VDE 0303
Dissipation Factor 0.035

@Frequency 50 Hz
0.035

@Frequency 50 Hz
0.035

@Frequency 1000 Hz
0.035

@Frequency 1000 Hz
0.048

@Frequency 1e+6 Hz
0.048

@Frequency 1e+6 Hz
Comparative Tracking Index >= 600 V
>= 600 V
DIN/IRC 112