Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

BASF Elastollan® 1195A Polyether Type Polyurethane Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP , Thermoplastic Polyurethane, Elastomer, Ether Grade
Manufacturer BASF
Trade Name Elastollan®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Elastollan® 1195A Polyether Type Polyurethane Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Processed by extrusion or injection molding. Elastollan ® 1100 series products are FDA Sec. 177.2600 compliant. Elastollan 1100 series of products are polyether-based thermoplastic polyurethanes. They exhibit excellent low temperature properties, hydrolysis resistance and fungus resistance. These products can be injection and blow molded and extruded. As with all TPU products this grade must be dried prior to processing.Property values below are typical values based on test samples cured 20 hours at 100°C before testing. Information provided by BASF Corporation.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 95
95
ASTM D2240
Hardness, Shore D 47
47
ASTM D2240
Tensile Strength, Ultimate 36.0 MPa
5220 psi
ASTM D412
Tensile Strength, Yield 12.0 MPa

@Strain 100 %
1740 psi

@Strain 100 %
ASTM D-412
21.0 MPa

@Strain 300 %
3050 psi

@Strain 300 %
ASTM D-412
Elongation at Break 490 %
490 %
ASTM D412
Modulus of Elasticity 0.0650 GPa
9.43 ksi
Shear Modulus 0.0390 GPa
5.66 ksi
Tear Strength 140 kN/m
799 pli
ASTM D624
Taber Abrasion, mg/1000 Cycles 55
55
H-18 wheel; ASTM D-1044.
Tensile Set 65 %
65 %
at break; ASTM D-412
Thermal Properties Metric English Comments
Vicat Softening Point 130 °C
266 °F
Electrical Properties Metric English Comments
Electrical Resistivity >= 1.00e+11 ohm-cm
>= 1.00e+11 ohm-cm
DIN 53482/VDE 0303
Surface Resistance >= 1.00e+11 ohm
>= 1.00e+11 ohm
DIN 53482/VDE 0303
Comparative Tracking Index >= 600 V
>= 600 V
DIN/IRC 112