BASF Elastollan S 60 A SPF TPUR

Category Polymer , Thermoplastic , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyester Grade
Manufacturer BASF
Trade Name Elastollan
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Elastollan S 60 A SPF TPUR.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applications: Shoe-soles, top pieces, tubes, technical parts e.g. castor tyres.Note: Quoted results are from measurements on injection molded test platens, post tempered for 20 hours at 100°CInformation provided by BASF
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ISO 1183-1-A
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
ISO 868
Tensile Strength 40.0 MPa
5800 psi
ISO 37
1.00 MPa

@Strain 20.0 %
145 psi

@Strain 20.0 %
ISO 37
2.40 MPa

@Strain 100 %
348 psi

@Strain 100 %
ISO 37
4.20 MPa

@Strain 300 %
609 psi

@Strain 300 %
ISO 37
Elongation at Break 850 %
850 %
ISO 37
Charpy Impact, Notched NB

@Temperature -30.0 °C
NB

@Temperature -22.0 °F
DIN EN ISO 179
NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
DIN EN ISO 179
Tear Strength 50.0 kN/m
285 pli
DIN ISO 34-1/Bb
Abrasion 30
30
[mm<sup>3</sup>; ISO 4649
Compression Set 25 %

@Temperature 23.0 °C
25 %

@Temperature 73.4 °F
ISO 815
40 %

@Temperature 70.0 °C
40 %

@Temperature 158 °F
ISO 815
Processing Properties Metric English Comments
Processing Temperature 175 - 220 °C
347 - 428 °F
Extrusion
175 - 240 °C
347 - 464 °F
Injection molding
Mold Temperature 20.0 - 70.0 °C
68.0 - 158 °F
Descriptive Properties Value Comments
Commercial Status North America
Primary Processing Technique Injection molding and Extrusion