Material Notes:
Formula: CH2NOCAS: 75-12-7Description: Formamide is a colorless liquid, with an odorless odor. It is miscible in water.Synonyms: MethanamideApplications: Intermediate used in the production of Crop protection, Pharmaceuticals, Pesticides, Industrial chemicals, Active ingredients and SolventInformation provided by BASF
Physical Properties Metric English Comments
Density 1.132 - 1.134 g/cc
0.04090 - 0.04097 lb/in³
DIN 51 757
Molecular Weight 45 g/mol
45 g/mol
Thermal Properties Metric English Comments
Melting Point 2.20 °C
36.0 °F
Boiling Point 210 °C
410 °F
Flash Point 175 °C
347 °F
Optical Properties Metric English Comments
Refractive Index 1.446 - 1.448
1.446 - 1.448
DIN 51 423
Processing Properties Metric English Comments
Moisture Content <= 0.050 %
<= 0.050 %
DIN 51 777
Descriptive Properties Value Comments
Assay >99%
Color absorbance 2.0 - 3.0°C
Composition Ammonium
<0.1%
Fe
<1.0 mg/l
Methanol
<0.1%
Ignition Temperature >500°C