BASF Isobutyl Acrylate

Category Fluid
Manufacturer BASF
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Isobutyl Acrylate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Formula: C7H12O2CAS: 106-63-8Description: Acrylic ester for manufacturing polymers and for use as a feedstock for syntheses. Applications: Isobutyl acrylate forms homopolymers and copolymers. Copolymers of isobutyl acrylate can be prepared with acrylic acid and its salts, amides and esters, and with methacrylates, acrylonitrile, maleic acid esters, vinyl acetate, vinyl chloride, vinylidene chloride, styrene, butadiene, unsaturated polyesters and drying oils, etc. Isobutyl acrylate is also a very useful feedstock for chemical syntheses, because it readily undergoes addition reactions with a wide variety of organic and inorganic compounds.Information provided by BASF
Physical Properties Metric English Comments
Density 0.890 g/cc
0.0322 lb/in³
Viscosity 0.80 cP
0.80 cP
[mPa.s]
Molecular Weight 128.2 g/mol
128.2 g/mol
Vapor Pressure 0.00880 bar
6.60 torr
Thermal Properties Metric English Comments
Specific Heat Capacity 1.90 J/g-°C
0.454 BTU/lb-°F
of Liquid
Melting Point -61.0 °C
-77.8 °F
Freezing Point
Boiling Point 139 °C
282 °F
Optical Properties Metric English Comments
Refractive Index 1.41
1.41
Processing Properties Metric English Comments
Moisture Content <= 0.10 %
<= 0.10 %
ASTM E203
Descriptive Properties Value Comments
Assay >99.5%
Color <20
ASTM D1209
Heat of Polymerization 535.1 kJ/kg
Latent Heat of Evaporation at Boiling Point 299.2 kJ/kg