BASF Lucalen® A 2710 H Ethylene/Acrylate Copolymer

Category Polymer , Thermoplastic , Ethylene Acrylic Acid
Manufacturer BASF
Trade Name Lucalen®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Lucalen® A 2710 H Ethylene/Acrylate Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product with properties which are typical of flexible PVC and of low density polyethylene. Suitable for flexible pipes, profiles and seals.Data was collected by ISO methods and provided by BASF.
Physical Properties Metric English Comments
Density 0.924 g/cc
0.0334 lb/in³
Water Absorption 0.050 %
0.050 %
Moisture Absorption at Equilibrium 0.050 %
0.050 %
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 14.0 MPa
2030 psi
Tensile Strength, Yield 4.00 MPa
580 psi
Elongation at Break >= 50 %
>= 50 %
Tensile Modulus 0.0450 GPa
6.53 ksi
Thermal Properties Metric English Comments
Melting Point 94.0 °C
201 °F
Electrical Properties Metric English Comments
Electrical Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
Dielectric Constant 2.8

@Frequency 1e+6 Hz
2.8

@Frequency 1e+6 Hz
Dissipation Factor 0.013

@Frequency 1e+6 Hz
0.013

@Frequency 1e+6 Hz