Material Notes:
Description: Lupranate® MP102 Isocyanate is a liquid, modified short chain prepolymer based on pure 4,4’-diphenylmethane diisocyanate (MDI). Lupranate MP102 Isocyanate is used in conjunction with high molecular weight and reactive polyether polyols for the manufacture of high-quality flexible and semi-flexible elastomers and integral skin foams. It is especially suitable for use in the manufacture of polyurethane shoe soles. For some semi-flexible and integral skin foam applications, Lupranate MP102 Isocyanate can be blended with polyisocyanates such as Lupranate M20 isocyanate. It is often used in mixtures with Lupranate MM103 isocyanate for large automotive moldings.Information provided by BASF
Physical Properties Metric English Comments
Density 1.21 g/cc
0.0437 lb/in³
Viscosity 700 cP
700 cP
Vapor Pressure 2.67e-7 bar

@Temperature 25.0 °C
0.000200 torr

@Temperature 77.0 °F
Thermal Properties Metric English Comments
Boiling Point >= 190 °C

@Pressure 0.000667 MPa
>= 374 °F

@Pressure 0.0967 psi
Flash Point >= 200 °C
>= 392 °F
Descriptive Properties Value Comments
Color Colorless
Composition Hydrolyzable Chlorine
<50.0%
NCO content
0.23