Material Notes:
Formula: C5H13NCAS: 996-35-0Description: Dimethylisopropanolamine is a colorless to yellow liquid with an amine-like odor. It is miscible in water.Synonyms: Dimethylisopropanolamine, 1-Dimethylamino-2-propanol, N,N-Dimethylamino-2-propanol, N,N-Dimethyl-2-hydroxypropylamineApplications: Intermediate used in the production of Dyes, Pharmaceuticals and Corrosion inhibitorInformation provided by BASF
Physical Properties Metric English Comments
Density 0.720 g/cc
0.0260 lb/in³
Molecular Weight 87.2 g/mol
87.2 g/mol
Thermal Properties Metric English Comments
Melting Point <= -70.0 °C
<= -94.0 °F
Boiling Point 65.0 - 67.0 °C
149 - 153 °F
Flash Point -27.0 °C
-16.6 °F
Processing Properties Metric English Comments
Moisture Content <= 0.50 %
<= 0.50 %
DIN 51 777
Descriptive Properties Value Comments
Assay >99%
Color <50
APHA, DIN EN 1557
Ignition Temperature 190°C