BASF Palatinol® 79P Linear Phthalate

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer BASF
Trade Name Palatinol®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Palatinol® 79P Linear Phthalate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Formula: C24H38O4Description: Palatinol 79P is a predominantly linear phthalate plasticizer based upon C7 and C9 alcohols. The ratio of these alcohols and their degree of linearity provide excellent processing characteristics, superior plastisol rheology and improved product flexibility under low temperature conditions when compared to DOP, DINP and DOTP in PVC resinsApplications: Palatinol 79P is a general purpose phthalate plasticizer and can replace DOP, DOTP and DINP in most applications; it can also replace general purpose blends that contain these plasticizers. Palatinol 79P exhibits better efficiency and imparts lower temperature flexibility than the above mentioned plasticizers. It is particularly useful in plastisol applications because it imparts lower initial viscosity, better viscosity and stability than branched plasticizers. Typical end uses are traffic cones, automotive sealants, fabric coating, fishing lures, extruded profiles and shoe compound.Information provided by BASF
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved