BASF Pluracol® 1603 Molded Foam Polyol

Category Fluid
Manufacturer BASF
Trade Name Pluracol®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Pluracol® 1603 Molded Foam Polyol.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Pluracol® 1603 polyol is a primary hydroxyl terminated polyether polyol containing an LVI inhibitor package making it ideal for molded seating foam applications. It has an actual functionality of 3.0. The high functionality and high primary content provide fast demold times and excellent stability in high water formulations. It can be used with Pluracol 1528FF graft poyol to formulate flexible foams with a wide range of hardnesses and densities.Information provided by BASF
Physical Properties Metric English Comments
Density 1.00 g/cc

@Temperature 55.0 °C
0.0361 lb/in³

@Temperature 131 °F
1.01 g/cc

@Temperature 40.0 °C
0.0365 lb/in³

@Temperature 104 °F
1.02 g/cc

@Temperature 25.0 °C
0.0368 lb/in³

@Temperature 77.0 °F
Viscosity 285 cP

@Temperature 55.0 °C
285 cP

@Temperature 131 °F
550 cP

@Temperature 40.0 °C
550 cP

@Temperature 104 °F
1202 cP

@Temperature 25.0 °C
1202 cP

@Temperature 77.0 °F
Chemical Properties Metric English Comments
Total Acid Number <= 0.060
<= 0.060
STI 3063/3161
Processing Properties Metric English Comments
Moisture Content <= 0.070 %
<= 0.070 %
STI 3062
Descriptive Properties Value Comments
Color <30
APHA, STI 3057
Clear Liquid
Composition Na & K
<11 ppm, STI 3038
Hydroxyl Number 29 - 33 mg KOH/g
STI 3007/3162
Unsaturation <0.07 meq/g
STI 3056