BASF Procom® GC20S 400 Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer BASF
Trade Name Procom®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Procom® GC20S 400 Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Uses: electrical appliance housings (e.g. drills), components requiring high impact and temperature resistance, furniture frames.Data was collected by ISO methods and provided by BASF.
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
Linear Mold Shrinkage, Flow 0.0060 cm/cm
0.0060 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 40.0 MPa
5800 psi
Elongation at Break 4.0 %
4.0 %
Tensile Modulus 3.60 GPa
522 ksi
Charpy Impact Unnotched 6.50 J/cm²
30.9 ft-lb/in²
5.00 J/cm²

@Temperature -30.0 °C
23.8 ft-lb/in²

@Temperature -22.0 °F
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 30.0 µm/m-°C

@Temperature 20.0 °C
16.7 µin/in-°F

@Temperature 68.0 °F
Deflection Temperature at 0.46 MPa (66 psi) 158 °C
316 °F
Deflection Temperature at 1.8 MPa (264 psi) 120 °C
248 °F
Vicat Softening Point 60.0 °C
140 °F