Material Notes:
Electrical and domestic appliances, housings where high gloss is required.Data was collected by ISO methods and provided by BASF.
Physical Properties Metric English Comments
Density 1.12 g/cc
0.0405 lb/in³
Linear Mold Shrinkage, Flow 0.0135 cm/cm
0.0135 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Yield 31.0 MPa
4500 psi
Elongation at Break 25 %
25 %
Tensile Modulus 2.30 GPa
334 ksi
Charpy Impact Unnotched 6.50 J/cm²
30.9 ft-lb/in²
1.50 J/cm²

@Temperature -30.0 °C
7.14 ft-lb/in²

@Temperature -22.0 °F
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 80.0 µm/m-°C

@Temperature 20.0 °C
44.4 µin/in-°F

@Temperature 68.0 °F
Deflection Temperature at 0.46 MPa (66 psi) 120 °C
248 °F
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °C
167 °F
Vicat Softening Point 100 °C
212 °F
Flammability, UL94 HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in