Material Notes:
Car bumpers and spoilers where good paintability is required.Data was collected by ISO methods and provided by BASF.
Physical Properties Metric English Comments
Density 0.930 g/cc
0.0336 lb/in³
Linear Mold Shrinkage, Flow 0.010 cm/cm
0.010 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Yield 15.0 MPa
2180 psi
Elongation at Break >= 50 %
>= 50 %
Tensile Modulus 0.850 GPa
123 ksi
Charpy Impact Unnotched NB
NB
23.0 J/cm²

@Temperature -30.0 °C
109 ft-lb/in²

@Temperature -22.0 °F
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 100 µm/m-°C

@Temperature 20.0 °C
55.6 µin/in-°F

@Temperature 68.0 °F
Deflection Temperature at 0.46 MPa (66 psi) 93.0 °C
199 °F
Deflection Temperature at 1.8 MPa (264 psi) 51.0 °C
124 °F
Vicat Softening Point 43.0 °C
109 °F