Material Notes:
Chemical Structure: Bismut-vanadium oxideApplication: Colourant for plastics; PVC-p, PVC-u, LD-PE, HD-PE, PP, PS, SB, SAN, PMMA and PARecommendations for food applications: BgVV, FrancePhysical form: PowderInformation provided by BASF
Physical Properties Metric English Comments
Bulk Density 0.800 g/cc
0.0289 lb/in³
Density 7.50 g/cc
0.271 lb/in³
pH 6.0
6.0
Specific Surface Area 8.0 m²/g
8.0 m²/g
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 300 °C
572 °F
Electrical Properties Metric English Comments
Electrical Resistivity 2350 ohm-cm
2350 ohm-cm
Descriptive Properties Value Comments
Chemical Fastness (months) H2SO4 10%
>6 months
H2SO4 conc.
>6 months
HCI 10%
>6 months
HCI conc.
>6 months
HNO3 10%
>6 months
HNO3 conc.
2 months
Na2CO3 sat.
>6 months
NaOH conc.
>6 months
Color Yellow
Light Fastness 8
Migration Fastness 5