BASF Styropor® P 240 EPS

Category Polymer , Thermoplastic , Polystyrene (PS) , Expanded Polystyrene (EPS)
Manufacturer BASF
Trade Name Styropor®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Styropor® P 240 EPS.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Expandable polystyrene (EPS) containing nominal 4.3 wt% pentane as the blowing agent.Intended uses: Shape molding of thick walled parts, including: High density applications (greater than 2.0 pcf); Fish boxes and coolers; and Low density, non-modified block with excellent regrind acceptability.Information provided by BASF
Physical Properties Metric English Comments
Bulk Density 0.0390 - 0.0400 g/cc
0.00141 - 0.00145 lb/in³
Density >= 0.900 g/cc
>= 0.0325 lb/in³
Descriptive Properties Value Comments
Commercial Status North America
Stabilization 50 sec
Steam time 3 - 5 sec