BASF Ultradur B 2300 G6 HR BK15116 30% Glass Filled PBT

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled
Manufacturer BASF
Trade Name Ultradur B
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Ultradur B 2300 G6 HR BK15116 30% Glass Filled PBT.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Ultradur B 2300 G6 HR BK15116 is a hydrolysis resistant, pigmented black 30% fiberglass reinforced PBT, exhibiting superior flow characteristics. Designed for improved latch strength in automotive connectors.
Physical Properties Metric English Comments
Density 1.52 g/cc
0.0549 lb/in³
ISO 1183
Viscosity Test 92 cm³/g
92 cm³/g
Viscosity number
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 140 MPa
20300 psi
5mm/min; ISO 527
Elongation at Break 3.2 %
3.2 %
5mm/min; ISO 527
Flexural Strength 212 MPa
30700 psi
ISO Data
Flexural Modulus 8.00 GPa
1160 ksi
ISO Data
Charpy Impact Unnotched 7.40 J/cm²
35.2 ft-lb/in²
ISO 179
Charpy Impact, Notched 1.10 J/cm²
5.24 ft-lb/in²
ISO 179
Thermal Properties Metric English Comments
Melting Point 223 °C
433 °F
10 K/min
223 °C
433 °F
ASTM Test
Descriptive Properties Value Comments
Color BK15116
Commercial Status North America and Europe
Impact Modified No
Primary Processing Technique Injection Molding