BASF Ultramid® 66 H2 G/25-V0KB1 BK 3324 PA66 (Dry)

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Glass Fiber Filled
Manufacturer BASF
Trade Name Ultramid®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Ultramid® 66 H2 G/25-V0KB1 BK 3324 PA66 (Dry).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Ultramid 66 H2 G/25-V0KB1 BK3324 is a 25% glass reinforced, heat stabilized injection molding grade. It's a V-0 self-extinguishing, with phosphorous. It offers good flowability, surface finish and good mechanical properties. It has excellent electrical properties.Information provided by BASF
Physical Properties Metric English Comments
Density 1.35 g/cc
0.0488 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 135 MPa
19600 psi
ISO 527
Elongation at Break 2.5 %
2.5 %
ISO 527
Flexural Modulus 7.50 GPa
1090 ksi
ISO 178
Izod Impact, Notched (ISO) 7.30 kJ/m²
3.47 ft-lb/in²
ISO 180
Charpy Impact, Notched 0.700 J/cm²
3.33 ft-lb/in²
ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 237 °C
459 °F
ISO 75
Processing Properties Metric English Comments
Melt Temperature 285 - 300 °C
545 - 572 °F
Mold Temperature 80.0 - 90.0 °C
176 - 194 °F
Dry Time 2 - 4 hour
2 - 4 hour
Moisture Content <= 0.050 %
<= 0.050 %
Descriptive Properties Value Comments
Color BK 3324
Commercial Status North America