BASF Ultramid® 8333G HI HS BK 106 33% Glass Filled PA6 (Conditioned)

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 30% Glass Fiber Filled
Manufacturer BASF
Trade Name Ultramid®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Ultramid® 8333G HI HS BK 106 33% Glass Filled PA6 (Conditioned).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description Ultramid 8333G HI HS BK-102 is a 33% glass reinforced, impact modified PA6 injection molding compound pigmented black developed for applications requiring improved dry as molded toughness in combination with a balance of strength, stiffness and excellent moldability/surface aesthetics.Applications: front wheel chair wheels, bicycle wheels, power tool housings, chain saw housings, clips and fasteners, hose clamps and window hardware.Information provided by BASF
Physical Properties Metric English Comments
Density 1.36 g/cc
0.0491 lb/in³
ASTM D792
Moisture Absorption at Equilibrium 0.90 %
0.90 %
24 hour; ASTM D570
1.5 %
1.5 %
50% RH; ASTM D570
5.5 %
5.5 %
Saturation; ASTM D570
Linear Mold Shrinkage 0.00762 cm/cm
0.00762 in/in
1/8" bar
Processing Properties Metric English Comments
Zone 1 245 - 275 °C
473 - 527 °F
Rear Zone
Zone 2 260 - 285 °C
500 - 545 °F
Center Zone
Zone 3 270 - 295 °C
518 - 563 °F
Front Zone
Zone 4 270 - 295 °C
518 - 563 °F
Nozzle
Melt Temperature 270 - 295 °C
518 - 563 °F
Mold Temperature 80.0 - 95.0 °C
176 - 203 °F
Dry Time 2 - 4 hour
2 - 4 hour
Moisture Content <= 0.080 %
<= 0.080 %
Descriptive Properties Value Comments
Color BK 106
Commercial Status North America
Users viewing this material also viewed the following: