BASF Ultramid® A3K Q603 PA66 (Conditioned)

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Unreinforced
Manufacturer BASF
Trade Name Ultramid®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Ultramid® A3K Q603 PA66 (Conditioned).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Ultramid A3K Q603 is a general purpose PA6/6.Information provided by BASF
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ISO 1183
Moisture Absorption at Equilibrium 2.5 %
2.5 %
50% RH; ISO 62
8.5 %
8.5 %
Saturation; ISO 62
Mechanical Properties Metric English Comments
Tensile Strength, Yield 54.0 MPa
7830 psi
ISO 527
Elongation at Break >= 50 %
>= 50 %
Nominal; ISO 527
Elongation at Yield 25 %
25 %
ISO 527
Tensile Modulus 1.20 GPa
174 ksi
ISO 527
Flexural Modulus 1.10 GPa
160 ksi
ISO 178
Izod Impact, Notched (ISO) 14.0 kJ/m²

@Temperature 23.0 °C
6.66 ft-lb/in²

@Temperature 73.4 °F
ISO 180
Charpy Impact Unnotched NB

@Temperature -30.0 °C
NB

@Temperature -22.0 °F
ISO 179
NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ISO 179
Charpy Impact, Notched 0.400 J/cm²

@Temperature -30.0 °C
1.90 ft-lb/in²

@Temperature -22.0 °F
ISO 179
1.60 J/cm²

@Temperature 23.0 °C
7.61 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Descriptive Properties Value Comments
Color Q603
Commercial Status North America