Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

BASF Ultramid® B3GM35 BK 60564 40% Glass/Mineral Filled PA6 (Dry)

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Glass/Mineral Reinforced
Manufacturer BASF
Trade Name Ultramid®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Ultramid® B3GM35 BK 60564 40% Glass/Mineral Filled PA6 (Dry).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Ultramid B3GM35 BK60564 is a 40% combined glass-fiber and mineral reinforced, pigmented black injection molding PA6 grade.Applications: industrial articles requiring medium rigidity and high dimensional stability.Information provided by BASF
Physical Properties Metric English Comments
Density 1.48 g/cc
0.0535 lb/in³
ISO 1183
Moisture Absorption at Equilibrium 1.7 %
1.7 %
50% RH; ISO 62
5.7 %
5.7 %
Saturation; ISO 62
Mechanical Properties Metric English Comments
Tensile Strength at Break 128 MPa
18600 psi
ISO 527
Elongation at Break 3.0 %
3.0 %
ISO 527
Tensile Modulus 8.30 GPa
1200 ksi
ISO 178
Flexural Modulus 7.55 GPa
1100 ksi
ISO 178
Izod Impact, Notched (ISO) 3.90 kJ/m²

@Temperature -40.0 °C
1.86 ft-lb/in²

@Temperature -40.0 °F
ISO 180
5.40 kJ/m²

@Temperature 23.0 °C
2.57 ft-lb/in²

@Temperature 73.4 °F
ISO 180
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
ISO 3146
Processing Properties Metric English Comments
Melt Temperature 270 - 295 °C
518 - 563 °F
Mold Temperature 80.0 - 95.0 °C
176 - 203 °F
Dry Time 2 - 4 hour
2 - 4 hour
Moisture Content <= 0.10 %
<= 0.10 %
Descriptive Properties Value Comments
Color BK 60564
Commercial Status North America