BASF Ultramid® B3WG6 BK00564 BGVW 30% Glass Filled PA6 (Conditioned)

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 30% Glass Fiber Filled
Manufacturer BASF
Trade Name Ultramid®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Ultramid® B3WG6 BK00564 BGVW 30% Glass Filled PA6 (Conditioned).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Ultramid B3WG6 BK00564 BGVW is a 30% glass fiber reinforced, pigmented black, heat stabilized injection molding PA6 grade.
Physical Properties Metric English Comments
Density 1.36 g/cc
0.0491 lb/in³
dry; ISO 1183
Water Absorption 2.1 %
2.1 %
24 hour; ISO Test
6.6 %
6.6 %
beginning dry; ISO 62
Moisture Absorption at Equilibrium 2.1 %
2.1 %
beginning dry (23°C/50% R.H.); ISO 62
Viscosity Test 140 cm³/g
140 cm³/g
Viscosity number
Linear Mold Shrinkage 0.0030 cm/cm
0.0030 in/in
ASTM Data; MD
Mechanical Properties Metric English Comments
Tensile Strength at Break 110 MPa
16000 psi
0.2 in/min; ASTM Test
Tensile Modulus 6.38 GPa
925 ksi
ASTM Test
Izod Impact, Notched 2.56 J/cm

@Thickness 3.17 mm
4.80 ft-lb/in

@Thickness 0.125 in
ASTM Test
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
10 K/min
220 °C
428 °F
ASTM Test
Descriptive Properties Value Comments
Color BK00564 BGVW
Commercial Status North America and Europe
Impact Modified No
Primary Processing Technique Injection Molding