BASF Ultramid® B3WG6 CR BK 23210 15% Glass Filled (Dry)

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 20% Glass Fiber Filled
Manufacturer BASF
Trade Name Ultramid®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Ultramid® B3WG6 CR BK 23210 15% Glass Filled (Dry).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Ultramid B3WG6 CR BK23210 s a 30% glass fiber reinforced, heat stabilized injection molding PA6 grade for crash relevant applications.Information provided by BASF
Physical Properties Metric English Comments
Density 1.36 g/cc
0.0491 lb/in³
ISO 1138
Moisture Absorption at Equilibrium 2.1 %
2.1 %
50% RH; ISO 62
6.6 %
6.6 %
Saturation; ISO 62
Melt Flow 40.8 g/10 min

@Load 5.00 kg,
Temperature 275 °C
40.8 g/10 min

@Load 11.0 lb,
Temperature 527 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 170 MPa
24700 psi
ISO 527
Elongation at Break 3.4 %
3.4 %
ISO 527
Tensile Modulus 9.50 GPa
1380 ksi
ISO 527
Charpy Impact Unnotched 9.50 J/cm²
45.2 ft-lb/in²
ISO 179
Charpy Impact, Notched 0.850 J/cm²

@Temperature -30.0 °C
4.04 ft-lb/in²

@Temperature -22.0 °F
ISO 179
1.25 J/cm²

@Temperature 23.0 °C
5.95 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 205 °C
401 °F
ISO 75
Descriptive Properties Value Comments
Color BK 23210
Commercial Status North America