BASF Ultramid® B3WGM 24 HP BK 23210 10/20% Glass/Mineral Filled PA6-1 (Conditioned)

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Glass/Mineral Reinforced
Manufacturer BASF
Trade Name Ultramid®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Ultramid® B3WGM 24 HP BK 23210 10/20% Glass/Mineral Filled PA6-1 (Conditioned).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: 20% mineral-filled and 10% glass-fiber reinforced injection-molding grade with outstanding flowability for technical parts with medium rigidity and high dimensional stability, e.g. for automotive engine covers, housings.Information provided by BASF
Physical Properties Metric English Comments
Density 1.37 g/cc
0.0495 lb/in³
ISO 1183
Water Absorption 6.9 - 7.5 %
6.9 - 7.5 %
Saturation; ISO 62
Moisture Absorption at Equilibrium 2.1 - 2.5 %
2.1 - 2.5 %
23°C; 50% RH; ISO 62
Viscosity Measurement 123
123
ISO 307
Melt Flow 116.45 g/10 min

@Load 5.00 kg,
Temperature 275 °C
116.45 g/10 min

@Load 11.0 lb,
Temperature 527 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 115 MPa
16700 psi
50 mm/min; ISO 527-1/-2
Elongation at Yield 5.0 %
5.0 %
50 mm/min; ISO 527-1/-2
Modulus of Elasticity 3.60 GPa
522 ksi
ISO 527-1/-2
Charpy Impact Unnotched 5.00 J/cm²

@Temperature 23.0 °C
23.8 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 1.50 J/cm²

@Temperature 23.0 °C
7.14 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Specific Heat Capacity 1.30 J/g-°C
0.311 BTU/lb-°F
Melting Point 220 °C
428 °F
DIN 53765
Maximum Service Temperature, Air 180 °C
356 °F
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+10 ohm-cm
1.00e+10 ohm-cm
IEC 60093
Surface Resistance 1.00e+10 ohm
1.00e+10 ohm
IEC 60093
Dielectric Constant 6.2

@Frequency 1.00 Hz
6.2

@Frequency 1.00 Hz
IEC 60250
Dissipation Factor 0.20

@Frequency 1.00e+6 Hz
0.20

@Frequency 1.00e+6 Hz
IEC 60250
Processing Properties Metric English Comments
Melt Temperature 250 - 290 °C
482 - 554 °F
Injection-molding/Extrusion
Mold Temperature 70.0 - 90.0 °C
158 - 194 °F
Injection-molding
Descriptive Properties Value Comments
Color BK 23210
Commercial Status Europe
Copyright © lookpolymers.com All Rights Reserved