Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

BASF Ultramid® BU50I PA6 (Conditioned)

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Unreinforced
Manufacturer BASF
Trade Name Ultramid®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Ultramid® BU50I PA6 (Conditioned).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Ultramid Ultratough Nylon BU50I is an unreinforced PA6, impact modified injection molding product that maintains its impact strength and ductility to -40 deg F (-40 deg C). The extreme low temperature tolerance of Ultratough Nylon BU50I makes it ideal for applications in which the weld line impact strength at low temperatures is critical.Applications: Automotive components, small engines, power tool parts and casings, cold weather and high impact supports gear, such as snowboards, ski components, helmets and hockey masks.Information provided by BASF
Physical Properties Metric English Comments
Density 1.06 g/cc
0.0383 lb/in³
ASTM D792
Moisture Absorption at Equilibrium 2.1 %
2.1 %
50% RH; ASTM D570
7.3 %
7.3 %
Saturation; ASTM D570
Linear Mold Shrinkage 0.04572 cm/cm
0.04572 in/in
1/8" bar
Processing Properties Metric English Comments
Melt Temperature 270 - 300 °C
518 - 572 °F
Mold Temperature 60.0 - 85.0 °C
140 - 185 °F
Dry Time 2 - 4 hour
2 - 4 hour
Moisture Content <= 0.15 %
<= 0.15 %
Descriptive Properties Value Comments
Commercial Status North America
Users viewing this material also viewed the following: