BASF Ultramid® N-276 BK ND 3007 40% Glass/Mineral Filled PA66

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Glass/Mineral Filled
Manufacturer BASF
Trade Name Ultramid®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Ultramid® N-276 BK ND 3007 40% Glass/Mineral Filled PA66.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Ultramid N-276 BK ND3007 is a 40% mineral/glass reinforced, heat stabilized injection molding PA6/6.Information provided by BASF
Physical Properties Metric English Comments
Density 1.50 g/cc
0.0542 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 135 MPa
19600 psi
ISO 527
Elongation at Break 3.0 %
3.0 %
ISO 527
Tensile Modulus 10.8 GPa
1570 ksi
ISO 527
Flexural Modulus 9.80 GPa
1420 ksi
ISO 178
Izod Impact, Notched (ISO) 4.20 kJ/m²
2.00 ft-lb/in²
ISO 180
Charpy Impact Unnotched 4.00 J/cm²

@Temperature -30.0 °C
19.0 ft-lb/in²

@Temperature -22.0 °F
ISO 179
4.50 J/cm²

@Temperature 23.0 °C
21.4 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Charpy Impact, Notched 0.350 J/cm²

@Temperature -30.0 °C
1.67 ft-lb/in²

@Temperature -22.0 °F
ISO 179
0.380 J/cm²

@Temperature 23.0 °C
1.81 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
ISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 255 °C
491 °F
ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 242 °C
468 °F
ISO 75
Processing Properties Metric English Comments
Melt Temperature 288 - 305 °C
550 - 581 °F
Mold Temperature 60.0 - 100 °C
140 - 212 °F
Injection Pressure 35.0 - 125 MPa
5080 - 18100 psi
Back Pressure 0.000 - 0.350 MPa
0.000 - 50.8 psi
Screw Speed 40 - 80 rpm
40 - 80 rpm
Descriptive Properties Value Comments
Color BK ND 3007
Commercial Status North America