Material Notes:
Ultrason E 2020 P is an unfilled, injection molding PES grade. Polyethersulfone flakes, for solvent based processes; product is soluble e.g. in N-Methylpyrrolidone and N,N-Dimethylacetamide.
Physical Properties Metric English Comments
Moisture Absorption at Equilibrium 1.0 %
1.0 %
23°C/50% R.H.; Equilibrium; ISO 62
Viscosity Test 56 cm³/g
56 cm³/g
Viscosity number
Mechanical Properties Metric English Comments
Tensile Strength at Break 90.0 MPa
13100 psi
5mm/min; ISO 527-2
Tensile Strength, Yield 90.0 MPa
13100 psi
50mm/min; ISO 527-2
Elongation at Break 6.7 %
6.7 %
5mm/min; ISO 527-2
Elongation at Yield 6.7 %
6.7 %
50mm/min; ISO 527-2
Tensile Modulus 2.70 GPa
392 ksi
ISO 527-2
Shear Modulus 0.200 GPa

@Temperature 225 °C
29.0 ksi

@Temperature 437 °F
ISO 6721
0.900 GPa

@Temperature 200 °C
131 ksi

@Temperature 392 °F
ISO 6721
0.950 GPa

@Temperature 100 °C
138 ksi

@Temperature 212 °F
ISO 6721
1.00 GPa

@Temperature 50.0 °C
145 ksi

@Temperature 122 °F
ISO 6721
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 205 °C
401 °F
ISO 75-2
Glass Transition Temp, Tg 225 °C
437 °F
10 K/min; ISO 11357-1/-2
Descriptive Properties Value Comments
Color Natural
Commercial Status North America and Europe
Impact Modified No
Primary Processing Technique Injection Molding