BCC Products BC 4544 Polyester Carvable Wood Filler

Category Polymer , Thermoset , Polyester, TS
Manufacturer BCC Products
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BCC Products BC 4544 Polyester Carvable Wood Filler.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This polyester resin base compound is easy to use, sets in minutes and can be sanded or carved almost immediately. Acts like wood yet exhibits no grain problems. BC4544 Wood Filler can be carved, sanded, filed, scraped, drilled, tapped or machined to a featheredge. No paint preparation is required and even accepts stain better than wood.APPLICATIONS: Tooling: A must for the wood tooling, model and pattern industry, making revisions, engineering changes and rebuilding of wood pattern and master models. Marine: Ideal for patching holes in hulls and bulkheads. An excellent water resistance item for emergency repairs for all types of wood and fiberglass boats. Furniture: For the restoration of all types of wood furniture and antiques. Seals and fills in holes, gouges and cracks. Great for the furniture refinisher. Other Applications: A unique lightweight filler paste designed for working with model craft and other wood products in any scale or form.Information provided by BCC Products, Inc.
Processing Properties Metric English Comments
Cure Time 20.0 - 60.0 min

@Temperature 24.0 °C
0.333 - 1.00 hour

@Temperature 75.2 °F
Pot Life 6.0 - 12 min

@Temperature 24.0 °C
6.0 - 12 min

@Temperature 75.2 °F
1lb mass
Shelf Life 12.0 Month
12.0 Month
in tightly closed container
Descriptive Properties Value Comments
Mix Ratio 100:1 or 100:2 resin/hardener