Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

BCC Products BC 5003 Epoxy Laminating System

Category Polymer , Thermoset , Epoxy
Manufacturer BCC Products
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BCC Products BC 5003 Epoxy Laminating System.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
BC 5003 is a medium viscosity, unfilled laminating system. It is a room temperature curing resin with a relatively short pot life. BC 5003 is also considered an excellent general purpose adhesive for in-shop use.Information provided by BCC Products, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.14 g/cc
1.14 g/cc
Brookfield Viscosity 3500 cP

@Temperature 23.9 °C
3500 cP

@Temperature 75.0 °F
Mixed
Mechanical Properties Metric English Comments
Hardness, Shore D 86
86
Tensile Strength, Ultimate 77.2 MPa
11200 psi
Flexural Strength 131 MPa
19000 psi
Flexural Modulus 3.31 GPa
480 ksi
Compressive Strength 116 MPa
16800 psi
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 77.8 °C
172 °F
Processing Properties Metric English Comments
Cure Time 360 - 480 min

@Temperature 24.0 °C
6.00 - 8.00 hour

@Temperature 75.2 °F
Pot Life 14 - 15 min

@Temperature 24.0 °C
14 - 15 min

@Temperature 75.2 °F
1/2 lb mass
Descriptive Properties Value Comments
Mix Ratio 100:20 by weight, 100:22 by volume, resin/harder