Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

BCC Products BC 5114 Epoxy Laminating System

Category Polymer , Thermoset , Epoxy
Manufacturer BCC Products
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BCC Products BC 5114 Epoxy Laminating System.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
BC 5114 is a gray low viscosity laminating system. This heat resistant resin exhibits excellent wet out, reasonable working time and may be used at room temperature without post-curing. For use above 150ºF a post-cure is required. BC 5114 can afford consistent use to 300ºF if required. Does not contain VCHD or MDA. Same uses as with BC 5105.Information provided by BCC Products, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.31 g/cc
1.31 g/cc
Brookfield Viscosity 3600 cP

@Temperature 23.9 °C
3600 cP

@Temperature 75.0 °F
Mechanical Properties Metric English Comments
Hardness, Shore D 90

@Temperature 23.9 °C
90

@Temperature 75.0 °F
Tensile Strength, Ultimate 179 MPa
26000 psi
10 oz glass cloth laminate
Flexural Strength 228 MPa
33000 psi
10 oz glass cloth laminate
Compressive Strength 364 MPa
52800 psi
10 oz glass cloth laminate
Thermal Properties Metric English Comments
CTE, linear 22.9 µm/m-°C
12.7 µin/in-°F
Deflection Temperature at 1.8 MPa (264 psi) 146 °C
295 °F
Processing Properties Metric English Comments
Cure Time 1440 min

@Temperature 24.0 °C
24.0 hour

@Temperature 75.2 °F
Pot Life 60 min

@Temperature 24.0 °C
60 min

@Temperature 75.2 °F
1 lb. mass
Descriptive Properties Value Comments
Mix Ratio 100:13 by weight, 100:18 by volume, resin/harder
Users viewing this material also viewed the following: