Material Notes:
BC 6060 is a blue epoxy, abrasion resistant surfacing resin. Commonly referred to as “die surface” material, this system may be applied by brush or if preferred, cast in thin sections to a maximum of ½”. Ideally suited for a variety of applications, BC 6060 is recommended for dies, foundry pattern and core boxes, router, trim and inspection fixtures.Information provided by BCC Products, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.76 g/cc
1.76 g/cc
Brookfield Viscosity 25000 cP

@Temperature 23.9 °C
25000 cP

@Temperature 75.0 °F
Mixed
Linear Mold Shrinkage 0.0020 cm/cm
0.0020 in/in
ASTM D2566-69
Mechanical Properties Metric English Comments
Hardness, Shore D 89

@Temperature 23.9 °C
89

@Temperature 75.0 °F
Tensile Strength, Ultimate 49.6 MPa
7200 psi
Flexural Strength 61.4 MPa
8900 psi
Compressive Strength 113 MPa
16400 psi
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °C
158 °F
Processing Properties Metric English Comments
Cure Time 720 - 960 min

@Temperature 24.0 °C
12.0 - 16.0 hour

@Temperature 75.2 °F
Pot Life 30 - 35 min

@Temperature 24.0 °C
30 - 35 min

@Temperature 75.2 °F
4 oz. mass
Descriptive Properties Value Comments
Machinability Poor
Mix Ratio 100:9 by weight, 100:15 by volume, resin/harder