Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

BCC Products BC 6126 Epoxy Surface Coat/Casting

Category Polymer , Thermoset , Epoxy
Manufacturer BCC Products
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BCC Products BC 6126 Epoxy Surface Coat/Casting.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
BC 6126 is a gray, low toxicity, aluminum filled, epoxy surface coat. This thixotropic resin system provides excellent surface duplication along with vertical coverage to 1/16 inch thickness. This heat resistant system may be used at room temperature without post-curing. For use above 150°F a post-cure is required. BC 6126 was engineered to replace VCHD and MDA systems while retaining excellent heat resistance. It is designed for consistent use up to 300°F.Uses: constructing vacuum form tools, RTM and RIM molds, compression and injection molds, and matched dies.Information provided by BCC Products, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.47 g/cc
1.47 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore D 90

@Temperature 23.9 °C
90

@Temperature 75.0 °F
Tensile Strength, Ultimate 40.0 MPa
5800 psi
Flexural Strength 44.8 MPa
6500 psi
Compressive Strength 193 MPa
28000 psi
Thermal Properties Metric English Comments
CTE, linear 42.5 µm/m-°C
23.6 µin/in-°F
Deflection Temperature at 1.8 MPa (264 psi) 144 °C
291 °F
Processing Properties Metric English Comments
Cure Time 960 min

@Temperature 24.0 °C
16.0 hour

@Temperature 75.2 °F
Pot Life 45 min

@Temperature 24.0 °C
45 min

@Temperature 75.2 °F
1 lb. mass
Descriptive Properties Value Comments
Mix Ratio 100:10 by weight, 100:15 by volume, resin/harder
Mixed Viscosity, Brookfield Thixotropic