Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

BCC Products BC 7053 Epoxy Casting

Category Polymer , Thermoset , Epoxy
Manufacturer BCC Products
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BCC Products BC 7053 Epoxy Casting.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
BC 7053 is an iron filled epoxy casting system. This system is a high iron content material that provides unsurpassed wear resistance. BC7053 was designed for use in constructing core boxes, holding and trimming fixtures, foundry patterns, etc.Information provided by BCC Products, Inc.
Physical Properties Metric English Comments
Specific Gravity 2.83 g/cc
2.83 g/cc
Brookfield Viscosity 10000 cP

@Temperature 23.9 °C
10000 cP

@Temperature 75.0 °F
Mixed
Linear Mold Shrinkage 0.00020 cm/cm
0.00020 in/in
ASTM D2566-69
Mechanical Properties Metric English Comments
Hardness, Shore D 90

@Temperature 23.9 °C
90

@Temperature 75.0 °F
Tensile Strength, Ultimate 49.6 MPa
7200 psi
Flexural Strength 62.1 MPa
9000 psi
Compressive Strength 106 MPa
15400 psi
Thermal Properties Metric English Comments
CTE, linear 57.6 µm/m-°C
32.0 µin/in-°F
Heat Distortion Temperature 52.8 °C
127 °F
Processing Properties Metric English Comments
Cure Time 720 - 1080 min

@Temperature 24.0 °C
12.0 - 18.0 hour

@Temperature 75.2 °F
10080 min

@Temperature 24.0 °C
168.0 hour

@Temperature 75.2 °F
complete cure
Pot Life 55 - 60 min

@Temperature 24.0 °C
55 - 60 min

@Temperature 75.2 °F
1 lb. mass
Descriptive Properties Value Comments
Machinability Good
Mix Ratio 100:5 by weight, 100:6.5 by volume, resin/harder
Copyright © lookpolymers.com All Rights Reserved