Material Notes:
New BC8010 is a quick setting urethane reproduction plastic system that simulates many of the desirable characteristics of aluminum metal. A highly machineable tooling material that is now easier to premix due to less settling. New BC8010 exhibits good heat transfer properties and is ideally suited for a multitude of applications, to include construction of short run low temperature vacuum form tools, prototypes, models, display parts, fixturing and bulk back fill.Information provided by BCC Products, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.75 - 1.85 g/cc
1.75 - 1.85 g/cc
Brookfield Viscosity 2250 cP

@Temperature 23.9 °C
2250 cP

@Temperature 75.0 °F
1 minute, #3 spindle @ 20 rpm
Linear Mold Shrinkage 0.00070 cm/cm
0.00070 in/in
ASTM D2566-69
Mechanical Properties Metric English Comments
Hardness, Shore D 83

@Temperature 23.9 °C
83

@Temperature 75.0 °F
Tensile Strength, Ultimate 27.90 MPa
4046 psi
ASTM D638
Flexural Strength 45.9 MPa
6650 psi
ASTM D790
Compressive Strength 67.2 MPa
9750 psi
ASTM D695
Thermal Properties Metric English Comments
Heat Distortion Temperature 81.7 °C
179 °F
Processing Properties Metric English Comments
Cure Time 90.0 - 120 min

@Temperature 24.0 °C
1.50 - 2.00 hour

@Temperature 75.2 °F
demold time
Pot Life 6.0 - 7.0 min

@Temperature 24.0 °C
6.0 - 7.0 min

@Temperature 75.2 °F
1 lb. mass
Descriptive Properties Value Comments
Mix Ratio 1:1 by weight or volume