Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Bapolene® 345F Medium Density Polyethylene Film Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer Bapolene®
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Bapolene® 345F Medium Density Polyethylene Film Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Bapolene 345F is a medium molecular weight film resin with excellent tensile, impact, and tear properties. Applications: Merchandise bags, produce and trash bags.Bapolene® and Bapolan® are registered trademarks of Bamberger Polymers, Inc. Information provided by Bamberger Polymers.
Physical Properties Metric English Comments
Density 0.936 g/cc
0.0338 lb/in³
ASTM D-1505
Thickness 25.0 microns
0.984 mil
4:1 blow-up ratio
Melt Flow 0.30 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.30 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
High Load Melt Index 20 g/10 min

@Load 21.6 kg,
Temperature 190 °C
20 g/10 min

@Load 47.6 lb,
Temperature 374 °F
HLMI; ASTM D1238
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 300 %
300 %
2 in/min; ASTM D-882
Film Elongation at Break, TD 780 %
780 %
2 in/min; ASTM D-882
Elmendorf Tear Strength, MD 15.0 g/micron
381 g/mil
ASTM D-1922
Elmendorf Tear Strength, TD 14.9 g/micron
377 g/mil
ASTM D-1922
Dart Drop 50.0 g/micron
1270 g/mil
26 in. dart; ASTM D-1709, A
Film Tensile Strength at Break, MD 52.0 MPa
7540 psi
2 in/min; ASTM D-882
Film Tensile Strength at Break, TD 38.0 MPa
5510 psi
2 in/min; ASTM D-882
Descriptive Properties Value Comments
Process Blown Film
Region Europe/Turkey
Bamberger Polymers Distribution
International
Bamberger Polymers Distribution
Mexico
Bamberger Polymers Distribution
US & Canada
Bamberger Polymers Distribution
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved