Material Notes:
Bapolene PP4062 is a high flow general purpose injection molding resin. This product meets FDA standards for food contact applications.Applications: Housewares, closures, spray caps, food containers, chairs, syringes, vials, pens, markers, knife handles, and toys.Bapolene® and Bapolan® are registered trademarks of Bamberger Polymers, Inc. Information provided by Bamberger Polymers
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D-1505
Melt Flow 12 g/10 min

@Load 2.16 kg,
Temperature 230 °C
12 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D-1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 99
99
ASTM D-785
Tensile Strength, Yield 33.8 MPa
4900 psi
ASTM D-638
Elongation at Yield 11 %
11 %
2 in/min (20 mm/min); ASTM D-638
Flexural Modulus 1.41 GPa
205 ksi
ASTM D-790
Izod Impact, Notched 0.320 J/cm
0.600 ft-lb/in
@23°; ASTM D-256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 101 °C
214 °F
ASTM D-648
Descriptive Properties Value Comments
Process Injection Molding
Region Europe/Turkey
Bamberger Polymers Distribution
International
Bamberger Polymers Distribution
Mexico
Bamberger Polymers Distribution
US & Canada
Bamberger Polymers Distribution
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved